Key takeaways Segregation in foamed concrete occurs when foam separates from the paste due to excess water, unstable foam, or improper mixing. The water-to-cement ratio and foam stability are the most critical factors affecting segregation. Always add foam after the base slurry is fully mixed, and use low-speed mixing for under 2 minutes. On-site controls …